Basic Info.
Model NO.
AlMn93%
Packing
Normal or Neutral-Packing
Transport Package
10kg/Bag
Specification
93%
Trademark
DongSheng
Origin
China
Production Capacity
2000mt/Month
Product Description
Aluminium alloying tablets
Application:
Used to ajust the content of Manganese,Iron,Chromium,Titanium,Copper or Nickel element in the manufacturer of high quality aluminium alloys.
Usage:
1. Tablets can be added directly to the melting furnace before refining , molten aluminum temperature required: 720-750 °C
2. Calculate addition amount of tablets.
3. Put tablets into molten aluminum dispersedly after skimming away the surface dross, close the furnace door and keep 10-20 minutes.
4. Stir completely for 10 minutes, refining for 15 minutes and drossing off to get needed alloy.
Alloying tablets:
Master alloys:
Others:
Product | Percentage of element | Specification |
Manganese tablet | Mn :75%,80%,85%,90%,93% | 1) Balance with pure Al powder or Non-hygroscopic(Sodium free) fluxes. 2) Size: Tablet: 500g-1333g/tablet. Mini-tablet:50g-200g/mini-tablet 3) Validity period: 8 months 4) Recovery rate >95% |
Iron tablet | Fe :75%,80%,85%,90%,97% | |
Titanium tablet | Ti : 75%,80%,85% | |
Chromium tablet | Cr :75%,80%,85% | |
Nickel tablet | Ni : 75%,80%,85% | |
Copper tablet | Cu :75%,80% | |
Fast melting Silicon | Si : 95% | |
Packaging | Tablet: 2-4 tablets wrapped with aluminium foil, 20kg/cardboard box, 1,000kg/plywood pallet. Mini-tablet: 10kg/paper bag , 1,000kg/plywood case. | |
Remark | Other weight and packaging can be produced upon customer's request. |
Application:
Used to ajust the content of Manganese,Iron,Chromium,Titanium,Copper or Nickel element in the manufacturer of high quality aluminium alloys.
Usage:
1. Tablets can be added directly to the melting furnace before refining , molten aluminum temperature required: 720-750 °C
2. Calculate addition amount of tablets.
3. Put tablets into molten aluminum dispersedly after skimming away the surface dross, close the furnace door and keep 10-20 minutes.
4. Stir completely for 10 minutes, refining for 15 minutes and drossing off to get needed alloy.
Alloying tablets:
Master alloys:
Others: