Ferro Niobium Lump 65%Min Nb for Smelting Superalloy

Application: Aviation, Electronics, Industrial
Standard: GB
Purity: 65%Min
Shape: Lump
Alloy: Alloy
Secondary: Non-secondary

Products Details

  • Overview
  • Product Description
  • Company Profile
  • FAQ
Overview

Basic Info.

Model NO.
Ferroniobium
Chemical Composition
Ferroalloy of Niobium and Iron
Melting Point
2467ºC
Feature
Has Solid Solution Strengthening and Carbide Preci
Transport Package
50kg / Iron Drum
Specification
10-50mm
Trademark
pusheng
Origin
Inner Mongolia
Production Capacity
1000 Tons/Month

Product Description

Product Description

Ferro Niobium Lump 65
 

FeNb ferro niobium ( Nb: 50% ~ 70%) .

 particle size:10-50mm & 50 mesh.60mesh... 325mesh

 

NIOBIUM - A material for innovations with great future potential
Niobium is a light gray metal with a gleaming white appearance on polished surfaces. It is characterized by a high melting point of 2,477°C and a density of 8.58g/cm³. Niobium can be easily formed, even at low temperatures. Niobium is ductile and occurs with tantalum in a natural ore. Like tantalum, niobium also features outstanding chemical and oxidation resistance.
 

Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy


Chemical composition%

 

 
chemical composition%
 
Brand
FeNb70
FeNb60-A
FeNb60-B
FeNb50-A
FeNb50-B
Nb+Ta
70-80
60-70
60-70
50-60
50-60
Ta
0.8
0.5
0.8
0.8
1.5
Al
3.8
2.0
2.0
2.0
2.0
Si
1.5
0.4
1.0
1.2
4.0
C
0.04
0.04
0.05
0.05
0.05
S
0.03
0.02
0.03
0.03
0.03
P
0.04
0.02
0.05
0.05
0.05
W
0.3
0.2
0.3
0.3
-
Ti
0.3
0.2
0.3
0.3
-
Cu
0.3
0.3
0.3
0.3
-
Mn
0.3
0.3
0.3
0.3
-
As
0.005
0.005
0.005
0.005
-
Sn
0.002
0.002
0.002
0.002
-
Sb
0.002
0.002
0.002
0.002
-
Pb
0.002
0.002
0.002
0.002
-
Bi
0.002
0.002
0.002
0.002
-
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Usage :

Ferroniobium is mainly used for smelting high temperature (heat resistant) alloy, stainless steel and high strength low alloy steel. Niobium forms stable niobium carbide with carbon in stainless steel and heat resistant steel. It can prevent the grain growth at high temperature, refine the structure of steel, and improve the strength, toughness and creep properties of steel.


 

Company Profile

Ferro Niobium Lump 65%Min Nb for Smelting Superalloy

Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy
Ferro Niobium Lump 65%Min Nb for Smelting Superalloy



Weclome to inner  mongolia pusheng iron& steel  Co,ltd
                                        

                                                                                         ----    a    partner    for   everything
company profile :
 

Since its establishment, Inner Mongolia Pusheng Iron and Steel Co., Ltd. has formed a nationwide sales network of ferroalloys and rare metals relying on the advantages of local resources. Main products: ferromanganese, ferrosilicon, metal manganese, metal silicon, magnesium ingot, ferrovanadium, ferromolybdenum, magnesium ingot, etc.

Pusheng people always adhere to the corporate culture of "people-oriented, scientific management, civilization and harmony, and pursuit of excellence", and strive to improve their own quality and promote professional management with the spirit of active learning, diligent thinking, courage to practice and good summary. in the primary position of enterprise development.

 
FAQ

Q: Are you a factory or a trading company?
We are factories and trading company.

Q: How to place order ?
A: Buyer send enquiry →get Pusheng Steel quotation → order confirmation→ Buyer arrange 30% deposit → Production started upon receipt of deposit→ Strict inspection during production → Buyer arrange balance payment
→ Packing → Delivery as per trade terms

Q: Can I have my own LOGO on the product?
Yes, you can send us your design and we can make your LOGO.

Q: Can you arrange the shipment?
Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.

Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .

Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.


Q: How long is your delivery time?
A: Generally it is 7-14 days if the goods are in stock. or it is 25-45 days if the goods are not in stock, it is according to
quantity.


Q:Can we get the some samples?Any charges?
A: Yes , we could offer the sample for free charge but do not pay the cost of freight . If you place the order after confirm the sample , we will refund your express freight or deducte it from the order amount .

Q: How do you make our business long-term and good relationship ?
A: 1.We keep good quality and competitive price to ensure our customers' benefit.
2.We respect every customer as our friend and we sincerrly do business and make friends with them, no matter where they come from.

Q: What is your terms of payment ?
A: 30% T/T deposit , 70% balance by T/T or L/C before shippment.

 

Contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours