CoCrW alloy is a range of cobalt-chromium alloys designed for wear resistance.
It is an entirely nonmagnetic and corrosion-resistant cobalt alloy.
There are several cobalt alloys with various compositions
optimized for different uses. Some are formulated to maximize combinations of wear resistance, corrosion resistance, or ability to withstand extreme temperatures.
1. Heat Resistance, wear resistance, corrosion resistance
2. Made as required dimensions and materials
3. Main products: valve seat, pump parts, pistons, bushings, nozzles etc
Brand and No | Carbon(Min-Max) | Manganese(Min-Max) | Silicon(Min-Max) | Chrome(Min-Max) | Nickel (Min-Max) | Moly (Min-Max) | Tung (Min-Max) | Cobalt(Min-Max) | Iron | Other |
CoCrW3 | 2.00-2.70 | 1.00 | 1.00 | 29.0-33.0 | 3.00 |
| 11.0-14.0 | Bal. | 3.00 | P.03MAX S.03MAX |
CoCrW4 | 1.00 | 1.00 | 1.5 | 28.0-32.0 | 3.00 | 1.50 | 12.5-15.5 | Bal. | 3.00 |
|
CoCrW6 | .90-1.4 | 1.00 | 1.5 | 27.0-31.0 | 3.00 | 1.50 | 3.50-5.50 | Bal. | 3.00 | P.04MAX S.04MAX |
Physical Properties
Item. | CoCrw3 | CoCrW6 | CoCrW12 | CoCrW394 | TTG25 | TTG25 | Blade (CFB) |
Hardness | 51-55 | 38-44 | 44-49 | 47-51 | 57-60 | 60-63 | 46.5-50 |
UNS R30006 Physical property (Room Temp.)
Density | Specific | Solidus | Liquidus | Specific heat | Magnetic | Electrode | Electrical | Electrical |
0.305 | 8.46 | 2340°F | 2540°F | 0.101°F | <1.2@200 | -0.25 | 1.9%IACS | 41.73 |
cobalt 6 Thermal Properties-Conductivity & Expansion
Thermal Expansion Coefficient | Thermal Conductivity by Temperature | ||||||
°F | Microinch/ | °C | Microns/ | °F | Btu/ft2/in/ | °C | W/mk |
212 | 6.3 | 100 | 11.34 | 70 | 102.7 | 21.11 | 14.82 |
Rod / Plate /Tube
International Exhibition in Chicago, Hanover
Our factory welcomes you to visit.
Our Services
1. Provide you with personalized service and professional technical guidance
2. According to the customer's use of the environment in different sizes and custom specifications
3. To ensure product quality and integrity of the service